物性表 |
||||||
性能項目 |
測試條件 |
測試方法 |
數(shù)值/描述 |
單位 |
||
機(jī)械性能 |
拉伸強(qiáng)度(引張強(qiáng)度) |
|
ASTM D638/ISO 527 |
83 |
kg/cm2(MPa)[Lb/in2] |
|
|
斷裂伸長率 |
|
ASTM D638/ISO 527 |
50 |
% |
|
|
拉伸模量 |
|
ASTM D638/ISO 527 |
|
kg/cm2(MPa)[Lb/in2] |
|
|
拉伸屈服伸長率(延伸率) |
|
ASTM D638/ISO 527 |
4 |
% |
|
|
拉伸斷裂伸長率(延伸率) |
|
ASTM D638/ISO 527 |
83 |
% |
|
|
彎曲模量(彎曲彈性率) |
|
ASTM D790/ISO 178 |
2800 |
kg·cm/cm(J/M)ft·lb/in |
|
|
彎曲強(qiáng)度 |
|
ASTM D790/ISO 178 |
|
kg·cm/cm(J/M)ft·lb/in |
|
|
洛氏硬度 |
|
ASTM D785 |
|
|
|
|
IZOD 缺口沖擊強(qiáng)度 |
1/4" 23℃ |
ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in |
|
|
|
1/4" -30℃ |
ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in |
|
|
|
1/8" 23℃ |
ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in |
|
|
|
1/8" -30℃ |
ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in |
|
|
Charpy沖擊強(qiáng)度 |
23℃ (缺口) |
ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in |
|
|
|
-30℃(缺口) |
ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in |
|
|
|
23℃(無缺口) |
ASTM D256/ISO 179 |
53 |
kg·cm/cm(J/M)ft·lb/in |
|
|
|
-30℃(無缺口) |
ASTM D256/ISO 179 |
105 |
kg·cm/cm(J/M)ft·lb/in |
|
物性性能 |
比重(密度) |
|
ASTM D792/ISO 1183 |
1.14 |
|
|
|
成型收縮率 |
|
ASTM D955 |
|
% |
|
|
熔融指數(shù)(流動系數(shù)) |
200℃/5kg |
ASTM D1238/ISO 1133 |
|
g/10min |
|
|
|
220℃/10kg |
ASTM D1238/ISO 1133 |
|
g/10min |
|
|
吸水率 23℃/24H |
|
ASTM D570/ISO 62 |
1.2 |
% |
大量供應(yīng)尼龍66塑膠原料